EFFECTS OF AGE-HARDENING AND WORK-HARDENING ON FRICTION AND WEAR OF AL-4 WT PERCENT CU DURING ABRASION

被引:14
|
作者
LIN, DS
WILMAN, H
机构
[1] Applied Physics and Chemistry, Surfaces Laboratory, Department of Chemical Engineering and Chemical Technology
关键词
D O I
10.1016/0043-1648(69)90013-1
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The friction, wear and surface microhardness of Al-4 wt. % Cu were measured during abrasion and their dependence on age-hardening and degree of work-hardening was investigated. New results are reported for the friction and wear behaviour of this alloy during age-hardening at different temperatures (~20, 165 and 250°C) and as a function of the degree of work-hardening. The (hardness, time) loci are substantially close to those of previous workers. The (friction, hardness) relationship is shown to be notably different for age-hardening and for work-hardening. The (wear resistance, hardness) loci for age-hardening appear to resemble in type those obtained by Khruschov in the case of abrasive wear of steels. The detailed analysis of the above data in terms of the calculated size and separation of the precipitate particles formed during ageing is presented in a later paper. © 1969.
引用
收藏
页码:323 / &
相关论文
共 50 条
  • [31] THE EFFECT OF WORK-HARDENING EXPONENT ON THE REMOVAL OF PLOUGHED METAL DURING ABRASIVE WEAR
    GARRISON, WM
    JOURNAL OF METALS, 1985, 37 (08): : A3 - A3
  • [32] EFFECT OF 0.5-PERCENT SILVER ON THE AGE-HARDENING BEHAVIOR OF AN AL-LI-CU-MG-ZR ALLOY
    ZHENG, ZQ
    LIANG, SQ
    XU, H
    TAN, CY
    YUN, DF
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1993, 12 (14) : 1111 - 1113
  • [33] Age-hardening characteristics of Al-Si-Cu-base cast alloys
    Kang, HG
    Kida, M
    Miyahara, H
    Ogi, K
    TRANSACTIONS OF THE AMERICAN FOUNDRYMEN'S SOCIETY, VOL 107, 1999, 107 : 507 - 515
  • [34] EFFECT OF RECOVERY TREATMENT ON RECRYSTALLIZATION OF AL-4 WT-PERCENT-CU
    CHANG, SK
    HUMPHREYS, FJ
    MATERIALS SCIENCE AND TECHNOLOGY, 1991, 7 (04) : 357 - 359
  • [35] LOW-TEMPERATURE DIFFUSION IN AL-7 WT PERCENT MG AND AL-4 WT PERCENT CU ALLOYS
    DOIG, P
    EDINGTON, JW
    PHILOSOPHICAL MAGAZINE, 1973, 28 (05): : 961 - 970
  • [36] THETA'-PHASE COALESCENCE IN AN AL-4 WT-PERCENT-CU ALLOY
    MERLE, P
    FOUQUET, F
    MERLIN, J
    SCRIPTA METALLURGICA, 1979, 13 (04): : 271 - 276
  • [37] Effect of iron addition on the work-hardening characteristics of Al-16wt% Ag alloy
    El-Salam, FA
    Mahmoud, MA
    El-Khalek, AMA
    Nada, RH
    PHYSICA B-CONDENSED MATTER, 2002, 324 (1-4) : 110 - 116
  • [38] EFFECTS OF CHANGES IN STRAIN PATH ON WORK-HARDENING IN CP ALUMINUM AND AN AL-CU-MG ALLOY
    WILSON, DV
    ZANDRAHIMI, M
    ROBERTS, WT
    ACTA METALLURGICA ET MATERIALIA, 1990, 38 (02): : 215 - 226
  • [39] AGE HARDENING OF MAGNESIUM ALLOY LA141A (MG + 14 WT PERCENT LI + 1 WT PERCENT AL)
    MCDONALD, JC
    ASM TRANSACTIONS QUARTERLY, 1968, 61 (03): : 505 - &
  • [40] Effect of Ag on age-hardening response of Al-Zn-Mg-Cu alloys
    Zhu, Qianqian
    Cao, Lingfei
    Wu, Xiaodong
    Zou, Yan
    Couper, Malcolm J.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 754 : 265 - 268