Tensile and oxidation behavior of SiC fibers

被引:0
|
作者
Cabet, C. [1 ]
Colin, C. [2 ]
Maxel, M. [2 ]
Robin, C. [1 ]
Gelebart, L. [2 ]
Bosonnet, S. [1 ]
Pasquier, S. [1 ]
Duprey, B. [1 ]
机构
[1] CEA, DEN, DPC, SCCME Lab Etud Corros Non Aqueuse, F-91191 Gif Sur Yvette, France
[2] CEA, DEN, DMN, SRMA Lab Etud Comportement Mecan Mat, F-91191 Gif Sur Yvette, France
来源
MATERIAUX & TECHNIQUES | 2011年 / 99卷 / 01期
关键词
Fiber; silicon carbide; tensile test; oxidation; fast reactor; helium;
D O I
10.1051/mattech/2011007
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In support of the development of SiC/SiC composite materials for fuel cladding in a Gas-cooled Fast Reactor, micrometric silicon carbide-based fibers with low residual oxygen were investigated in the reactor operating environment. A dedicated machine enabled to slow tensile strain single fibers from room temperature up to 1700 degrees C under secondary vacuum. It was observed that fibers are brittle and their mechanical properties drop when the temperature is increased. In addition, thermogravimetric analysis was performed at 1100 degrees C under helium with an oxygen partial pressure of 20 Pa. Fibers oxidized and the reaction rate appeared to be globally parabolic after about 60 h. Electronic microscopy confirmed that a thin silicon-oxide scale has been formed on the fiber surface. Future work includes studying the effect of oxidation on the fiber tensile behavior.
引用
收藏
页码:121 / 125
页数:5
相关论文
共 50 条
  • [21] Effect of CVI SiC interphase on tensile properties of SiC fibers with different surfaces
    Lv, Xiaoxu
    Sun, Jiajia
    Liu, Wei
    Yang, Jinhua
    Jiao, Jian
    VACUUM, 2023, 216
  • [22] Processing, sintering and oxidation behavior of SiC fibers reinforced ZrB2 composites
    Sciti, Diletta
    Silvestroni, Laura
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2012, 32 (09) : 1933 - 1940
  • [23] Oxidation behavior of short SiC fibers-reinforced glass-ceramic composites
    Gao, Jiqiang
    Huang, Qingwei
    Wu, Yahong
    Yin, Xiaodong
    Jin, Zhihao
    Hsi-An Chiao Tung Ta Hsueh/Journal of Xi'an Jiaotong University, 1999, 33 (02): : 38 - 40
  • [24] Role of SiC nanowire coating on oxidation behavior of carbon fibers: Kinetic and thermodynamic study
    Prakash, Jyoti
    Dasgupta, Kinshuk
    Kumar, Brij
    Ghosh, Sunil Kumar
    Chakravartty, J. K.
    SURFACE & COATINGS TECHNOLOGY, 2014, 259 : 637 - 646
  • [25] Tensile properties and creep behavior of SiC-based fibers under various oxygen partial pressures
    Sha, JJ
    Park, JS
    Hinoki, T
    Kohyama, A
    Yu, J
    PRICM 5: THE FIFTH PACIFIC RIM INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS AND PROCESSING, PTS 1-5, 2005, 475-479 : 1333 - 1336
  • [26] Effect of heat treatment on microstructure and tensile strength of KD-II SiC fibers in argon and oxidation atmosphere
    Yin, Huan
    Yang, Fenghao
    Hu, Guangmin
    Yi, Maozhong
    JOURNAL OF CERAMIC PROCESSING RESEARCH, 2023, 24 (04): : 742 - 752
  • [27] Oxidation embrittlement of SiC fibers at intermediate temperatures
    Mazerat, S.
    El-Morsli, J.
    Sarrazin, R.
    Pailler, R.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2024, 44 (07) : 4465 - 4481
  • [28] Tensile fracture Behavior of Nicalon/SiC composites
    Kim, Jeongguk
    Liaw, P. K.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2007, 38A (13): : 2203 - 2213
  • [29] Tensile Fracture Behavior of Nicalon/SiC Composites
    Jeongguk Kim
    P.K. Liaw
    Metallurgical and Materials Transactions A, 2007, 38 : 2203 - 2213
  • [30] SYNTHESIS OF CONTINUOUS SIC FIBERS WITH HIGH-TENSILE STRENGTH
    YAJIMA, S
    OKAMURA, K
    HAYASHI, J
    OMORI, M
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1976, 59 (7-8) : 324 - 327