共 50 条
[41]
KINETICS OF RECOVERY OF COLD-WORKED METALS FROM INTERNAL-FRICTION AND ELASTICITY MEASUREMENTS - REPLY
[J].
JOURNAL OF THE INSTITUTE OF METALS,
1959, 87 (08)
:154-154
[43]
INFLUENCE OF ALLOYAGE ON 200DEGREES PEAK OF INTERNAL-FRICTION IN COLD-WORKED STEEL
[J].
FIZIKA METALLOV I METALLOVEDENIE,
1976, 42 (03)
:578-582
[44]
ELASTIC-MODULI AND INTERNAL-FRICTION OF COLD-WORKED COPPER SINGLE-CRYSTALS
[J].
ACTA METALLURGICA,
1975, 23 (07)
:783-792
[45]
ANOMALOUS INTERNAL-FRICTION PEAKS IN COLD-WORKED DILUTE AL-MG ALLOYS
[J].
MATERIALS SCIENCE AND ENGINEERING,
1981, 49 (02)
:101-107
[46]
INTERNAL-FRICTION STUDY ON THE STRUCTURE CHANGE OF COLD-WORKED METALS ANNEALED AT VARIOUS TEMPERATURES
[J].
JOURNAL DE PHYSIQUE,
1985, 46 (C-10)
:351-354
[47]
STUDY OF RECRYSTALLIZATION OF WORKHARDENED 99.998 PERCENT PURITY SILVER BY MEASURING INTERNAL-FRICTION AND MODULUS DEFECT IN KHZ RANGE
[J].
MEMOIRES SCIENTIFIQUES DE LA REVUE DE METALLURGIE,
1972, 69 (03)
:223-&
[48]
ON INTERNAL-FRICTION AND YOUNG MODULUS DEFECT DURING CRYSTAL DEFORMATION
[J].
FIZIKA TVERDOGO TELA,
1992, 34 (09)
:2915-2921
[49]
INTERNAL-FRICTION PEAKS OF COLD-WORKED CU + 0.1 AT-PERCENT AG IN THE KHZ RANGE
[J].
ACTA METALLURGICA,
1980, 28 (07)
:855-868
[50]
INTERNAL-FRICTION PEAK IN UN-RECRYSTALLIZED COLD-WORKED HIGH-PURITY METALS
[J].
SCRIPTA METALLURGICA,
1988, 22 (04)
:539-544