SYNTHESIS OF HIGH-TC 2223 PHASE IN BI-PB-SR-CA-CU-O SYSTEM BY SHORT-TERM FIRING

被引:0
|
作者
SHIMONO, I
KONISHI, H
KIJIMA, N
NAGATA, S
机构
[1] SHINSHU UNIV, FAC TEXT SCI & TECHNOL, UEDA, NAGANO 386, JAPAN
[2] MURORAN INST TECHNOL, MURORAN, HOKKAIDO 050, JAPAN
来源
NIPPON SERAMIKKUSU KYOKAI GAKUJUTSU RONBUNSHI-JOURNAL OF THE CERAMIC SOCIETY OF JAPAN | 1994年 / 102卷 / 06期
关键词
SUPERCONDUCTOR; BI-PB-SR-CA-CU-O; 2223; PHASE; SOLID-STATE REACTION;
D O I
暂无
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The high-T(c) 2223 phase in the Bi-Pb-Sr-Ca-Cu-O system has been synthesized by solid-state reaction. The processing parameters which give the largest volume fraction of the 2223 phase were found as follows. A mixture of Bi2O3, PbO, SrCO3, CaCO3 and CuO was pressed into a bar-shape and calcined at 1133 K for 5h, then cooled to 873 K with a cooling rate of 0.5 K/min. After being pulverized and pressed, the specimen was fired again at 1133 K for 5h and cooled to 873 K with a cooling rate of 0.5 K/min. With these simple synthesizing procedures, a superconducting sample which has a high T(c)-2223 phase volume fraction as high as. 91%, was successfully obtained. Our synthesizing method results in a much greater volume fraction of the 2223 phase than do conventional methods. The zero-resistance temperature of our sample was 102 K.
引用
收藏
页码:606 / 608
页数:3
相关论文
共 50 条
  • [1] DIFFUSION BONDING OF BI-PB-SR-CA-CU-O HIGH-TC SUPERCONDUCTORS
    MUTOH, Y
    INOUE, M
    KOMATSU, T
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 2-LETTERS & EXPRESS LETTERS, 1990, 29 (08): : L1432 - L1434
  • [2] Rapid formation of high Tc phase in Bi-Pb-Sr-Ca-Cu-O system
    Mancic, L
    Milosevic, O
    Marinkovic, B
    Lopez, MDD
    Rizzo, F
    PHYSICA C-SUPERCONDUCTIVITY AND ITS APPLICATIONS, 2000, 341 : 503 - 504
  • [3] Formation process of 2223 phase in Bi-Pb-Sr-Ca-Cu-O system via calcining at 1073 K
    Shimono, I
    Kijima, N
    Nagata, S
    Konishi, H
    Hamaguchi, Y
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1996, 104 (02) : 101 - 108
  • [4] EFFECT OF BI PB RATIO AND ANNEALING TEMPERATURE ON TC AND FORMATION OF HIGH-TC PHASE IN BI-PB-SR-CA-CU-O SUPERCONDUCTOR
    XI, ZP
    JI, CL
    ZHOU, L
    JOURNAL OF SUPERCONDUCTIVITY, 1990, 3 (04): : 421 - 423
  • [5] SINGLE (2223) PHASE AND TRANSPORT CURRENT PATH IN BI-PB-SR-CA-CU-O
    OOTA, A
    OHBA, K
    ISHIDA, A
    NOJI, H
    KIRIHIGASHI, A
    IWASAKI, K
    KUWAJIMA, H
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 2-LETTERS & EXPRESS LETTERS, 1990, 29 (02): : L262 - L265
  • [6] LARGE VESSELS OF HIGH-TC BI-PB-SR-CA-CU-O SUPERCONDUCTOR FOR MAGNETIC-SHIELD
    HOSHINO, K
    OHTA, H
    SUDOH, E
    KATOH, K
    YAMAZAKI, S
    TAKAHARA, H
    AONO, M
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 2-LETTERS, 1990, 29 (08): : L1435 - L1438
  • [7] PREPARATION OF BI-PB-SR-CA-CU-O SUPERCONDUCTOR BY THE CITRATE METHOD
    SHIMONO, I
    NAGATA, S
    KONISHI, H
    HAMAGUCHI, Y
    NIPPON SERAMIKKUSU KYOKAI GAKUJUTSU RONBUNSHI-JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1993, 101 (09): : 1044 - 1050
  • [8] Mechanochemical Effects on Synthesis of Bi-Pb-Sr-Ca-Cu-O Superconductor
    李希明
    淡野正信
    Rare Metals, 1997, (04) : 37 - 43
  • [9] EFFECTS OF SR/CA RATIO AND CUO CONTENT OF THE SUPERCONDUCTING PHASES IN THE BI-PB-SR-CA-CU-O SYSTEM
    XI, ZP
    ZHOU, L
    JI, CL
    WU, XZ
    JOURNAL OF SUPERCONDUCTIVITY, 1991, 4 (06): : 455 - 459
  • [10] PRESSURE-EFFECT STUDY ON THE HIGH-TC SUPERCONDUCTOR BI(PB)-SR-CA-CU-O SYSTEM
    YONEDA, T
    MORI, Y
    AKAHAMA, Y
    KOBAYASHI, M
    KAWAMURA, H
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 2-LETTERS & EXPRESS LETTERS, 1990, 29 (08): : L1396 - L1398