共 50 条
- [41] RETRACTED: Role of hydrogen environment induced hydrogen embrittlement of Ti-8Al-1Mo-2V alloy (Retracted article. See vol. 556, pg. 985, 2012) MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 494 (1-2): : 143 - 146
- [42] HIGH-STRENGTH ALLOYS UNDER STRESS IN CORROSIVE ENVIRONMENTS (EFFECT OF SPECIMEN BREADTH ON SUSCEPTIBILITY TO STRESS-CORROSION CRACKING OF TI8AL-1MO-1V ALLOY IN SALT WATER) REPORT OF NRL PROGRESS, 1967, (AUG): : 45 - &
- [43] STUDIES ON HYDROGEN EMBRITTLEMENTS OF A 3CR-1MO-1/4V-TI-B PRESSURE-VESSEL STEEL .1. EVALUATIONS OF THE RESISTANCE TO HYDROGEN EMBRITTLEMENT TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1985, 71 : 1304 - 1304
- [44] EFFECT OF HYDROGEN CONTENT ON SUSTAINED-LOAD CLEAVAGE CRACKING OF TI-8A1-1MO-1V IN VACUUM REPORT OF NRL PROGRESS, 1970, (SEP): : 30 - &
- [46] THE EFFECT OF INTERNAL HYDROGEN ON THE STRESS-CORROSION CRACKING OF TI-6AL-6V-2SN IN 3.5-PERCENT NACL SOLUTION MATERIALS SCIENCE AND ENGINEERING, 1980, 45 (01): : 49 - 54
- [47] STUDIES ON HYDROGEN EMBRITTLEMENTS OF A 3CR-1MO-1/4V-TI-B PRESSURE-VESSEL STEEL .2. METALLURGICAL FACTORS AFFECTING THE HYDROGEN EMBRITTLEMENT TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1985, 71 : 1305 - 1305
- [50] Effect of hydrogen charging on microstructural evolution and corrosion behavior of Ti-4Al-2V-1Mo-1Fe alloy JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2021, 60 : 168 - 176