GRAIN-BOUNDARY REACTION IN A CU-10 MASS-PERCENT-NI-8MASS-PERCENT-SN ALLOY

被引:6
作者
MIKI, M
SOGABE, T
HORI, S
机构
[1] OSAKA UNIV, FAC ENGN, OSAKA, JAPAN
[2] NIIHAMA TECH COLL, NIIHAMA, JAPAN
关键词
All Open Access; Bronze;
D O I
10.2320/jinstmet1952.46.3_307
中图分类号
学科分类号
摘要
COPPER NICKEL TIN ALLOYS
引用
收藏
页码:307 / 312
页数:6
相关论文
共 14 条
[1]   INITIAL-STAGES OF DECOMPOSITION IN CU-9NI-6SN [J].
BABURAJ, EG ;
KULKARNI, UD ;
MENON, ESK ;
KRISHNAN, R .
JOURNAL OF APPLIED CRYSTALLOGRAPHY, 1979, 12 (OCT) :476-480
[2]  
BASTOW BD, 1971, J I MET, V99, P277
[3]   DIFFRACTION STUDY OF SPINODAL DECOMPOSITION IN CU-10 W-O NI-6 W-O SN [J].
DITCHEK, B ;
SCHWARTZ, LH .
ACTA METALLURGICA, 1980, 28 (06) :807-822
[4]  
HORNBOGEN E, 1972, MET T, V3, P2712
[5]  
Johnson WA, 1939, T AM I MIN MET ENG, V135, P416
[6]   TEMPERATURE-DEPENDENCE OF YIELD STRESS AND WORK-HARDENING IN SPINODALLY DECOMPOSED CU-10NI-6SN ALLOY [J].
KATO, M ;
SCHWARTZ, LH .
MATERIALS SCIENCE AND ENGINEERING, 1979, 41 (01) :137-142
[7]   AGE HARDENING IN CU-15NI-8SN ALLOY [J].
LEFEVRE, BG ;
DANNESSA, AT ;
KALISH, D .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1978, 9 (04) :577-586
[8]  
PETERMANN J, 1968, Z METALLKD, V59, P814
[9]   HIGH-STRENGTH CU-NI-SN ALLOYS BY THERMOMECHANICAL PROCESSING [J].
PLEWES, JT .
METALLURGICAL TRANSACTIONS, 1975, A 6 (03) :537-544
[10]  
Price WB, 1928, T AM I MIN MET ENG, V78, P503