共 23 条
- [1] BEACHEM CD, 1965, T ASME D, V87, P299
- [2] Bernstein I. M., 1976, International Metals Reviews, V21, P269
- [3] Bernstein I.M., 1976, EFFECT HYDROGEN BEHA, P37
- [4] TEMPERED MARTENSITE EMBRITTLEMENT IN A HIGH-PURITY STEEL [J]. METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1979, 10 (08): : 1151 - 1155
- [5] ROLE OF HYDROGEN IN THE DUCTILE FRACTURE OF PLAIN CARBON-STEELS [J]. METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1979, 10 (03): : 367 - 375
- [6] HYDROGEN ASSISTED DUCTILE FRACTURE OF SPHEROIDIZED CARBON-STEELS [J]. METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1981, 12 (02): : 225 - 234
- [7] EFFECT OF HYDROGEN ON DUCTILE FRACTURE OF SPHEROIDIZED STEEL [J]. SCRIPTA METALLURGICA, 1976, 10 (04): : 341 - 345
- [8] DUCTILE FRACTURE OF U-NOTCHED BEND SPECIMENS OF SPHEROIDIZED AISI-1095 STEEL [J]. METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1978, 9 (11): : 1663 - 1671