THERMAL-DEGRADATION OF POLYIMIDES .2. MECHANISM OF CARBON-DIOXIDE FORMATION DURING THERMAL-DEGRADATION

被引:17
作者
ZURAKOWSKAORSZAGH, J [1 ]
CHREPTOWICZ, T [1 ]
机构
[1] SCH MED,DEPT INORGAN & ANALYT CHEM,PL-02097 WARSAW,POLAND
关键词
D O I
10.1016/0014-3057(81)90192-0
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
引用
收藏
页码:877 / 880
页数:4
相关论文
共 10 条
  • [1] Bruck S.D., 1965, POLYMER, V6, P49
  • [2] DOUGLAS H, 1953, CAN J CHEM, V31, P1127
  • [3] ENDREY AL, 1962, Patent No. 645073
  • [4] SUCCINIMIDYL RADICAL PROBLEM . EASE OF FORMATION OF NITROGEN AND OXYGEN PI AND SIGMA FREE RADICALS
    HEDAYA, E
    HINMAN, RL
    SCHOMAKE.V
    THEODORO.S
    KYLE, LM
    [J]. JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 1967, 89 (19) : 4875 - &
  • [5] THERMAL DECOMPOSITION OF POLYIMIDES IN VACUUM
    JOHNSTON, TH
    GAULIN, CA
    [J]. JOURNAL OF MACROMOLECULAR SCIENCE-CHEMISTRY, 1969, A 3 (06): : 1161 - &
  • [6] KRASNOV EP, 1970, VYSOKOMOL SOEDIN A, V12, P873
  • [7] KROMAITE P, 1972, VYSOKOMOLEK SOEDIN A, V15, P148
  • [8] OKSENTEVITCH L, 1977, VYSOKOMOLEK SOEDIN A, V3, P553
  • [9] TELESHOV.AS, 1971, VYSOKOMOL SOEDIN A, V13, P2309
  • [10] THERMAL-DEGRADATION OF POLYIMIDES .1. INVESTIGATION OF THE ROLE OF ISOIMIDE STRUCTURE ON DEGRADATION PROCESS
    ZURAKOWSKAORSZAGH, J
    CHREPTOWICZ, T
    ORZESZKO, A
    KAMINSKI, J
    [J]. EUROPEAN POLYMER JOURNAL, 1979, 15 (04) : 409 - 413