[31]
ALLOY OF 20 PERCENT COPPER, 20 PERCENT NICKEL AND 20 PERCENT MANGANESE AT CRITICAL-TEMPERATURE
[J].
PHYSICA STATUS SOLIDI A-APPLICATIONS AND MATERIALS SCIENCE,
1972, 11 (02)
:K131-+
[33]
TENSILE PROPERTIES OF TEMPERED CHROMIUM STEELS IN TEMPERATURE-RANGE 0 DEGREES TO 700 DEGREES C
[J].
METALLURGICAL TRANSACTIONS,
1972, 3 (04)
:953-+
[34]
SPINODAL DECOMPOSITION AND MECHANICAL-PROPERTIES OF AN AUSTENITIC FE-30WT-PERCENT-MN-9WT-PERCENT-AL-0.9WT-PERCENT-C ALLOY
[J].
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING,
1989, 111
:45-50
[35]
DEFORMATION BEHAVIOR OF A1-80 WT PERCENT ZN ALLOY AT TEMPERATURES BETWEEN 25 DEGREES C TO 320 DEGREES C
[J].
JOURNAL OF METALS,
1968, 20 (01)
:A66-&
[36]
DILATOMETRIC EFFECTS OF HARDENING AND RECRYSTALLIZATION IN THE 60 COPPER-20 NICKEL-20 MANGANESE ALLOY
[J].
TRANSACTIONS OF THE AMERICAN SOCIETY FOR METALS,
1949, 41
:961-984
[38]
FULL-AUSTENITE CHROMIUM-NICKEL-MOLYBDENUM STEELS CONTAINING ABOUT 0.03 PERCENT C AND 0.1 PERCENT N FOR USE WITHIN TEMPERATURE-RANGE OF - 269 TO 700 DEGREES C
[J].
STAHL UND EISEN,
1972, 92 (09)
:393-&
[39]
KINETICS OF NICKEL SULFIDATION AT 560-600-DEGREES-C
[J].
JOURNAL OF METALS,
1985, 37 (11)
:A28-A28
[40]
THE SULFIDATION OF MANGANESE AT LOW SULFUR PRESSURES AT 700-950-DEGREES-C
[J].
OXIDATION OF METALS,
1991, 35 (3-4)
:175-198