Compressive Strength of Steel-Fiber Concrete with Artificial Lightweight Aggregate (ALWA)

被引:4
作者
Wulandari, Meity [1 ]
Tavio [1 ]
Raka, I. G. P. [1 ]
Puryanto [2 ]
机构
[1] Inst Teknol Sepuluh Nopember ITS, Dept Civil Engn, Surabaya 60111, Indonesia
[2] Politekn Negeri Sriwijaya, Dept Civil Engn, Palembang 30139, Indonesia
来源
CIVIL ENGINEERING JOURNAL-TEHRAN | 2018年 / 4卷 / 09期
关键词
Artificial Lightweight Aggregate (ALWA); Compressive Strength; Density; Modulus of Elasticity; Steel Fibers; Styrofoam;
D O I
10.28991/cej-03091134
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
In the last decade, there have been many innovations developed to replace the aggregate as material for concrete, particularly the coarse aggregate using the artificial lightweight aggregates a.k.a. ALWA. In the study, the main ingredient used to develop the artificial lightweight aggregates is the styrofoam. Styrofoam has a lightweight characteristic so that it can reduce the density of the concrete. If the density of the concrete can be lighter than the normal-weight concrete then the overall weight of the structure of a building will also be lighter. Thus, the shear force due to the earthquake will also be smaller so that the safety of the building becomes better. The styrofoam used was dissolved with the acetone solution and formed into granules in which the size resembled the coarse aggregate size of about 10 to 20 mm. The styrofoam which has been formed then dried up so that the texture becomes hard. In addition, steel fiber was also used as an added ingredient in concrete mixtures so that the concrete was highly resistant against cracking and was expected to increase the compressive strength of the concrete. ALWA compositions used to replace coarse aggregates were 0%, 15%, 50%, and 100%. While the composition of steel fiber used was 0%, 0.75%, and 1.5% of the total volume of the cylinder. The type of steel fiber used was hooked-end steel fiber with the diameter and the length of 0.8 mm and 60 mm, respectively. The results showed that the concrete with 15% styrofoam ALWA and 1.5% of steel fiber were able to produce optimum compressive strength by 28.5 NfPa and the modulus of elasticity by 23,495 MPa. In addition, the use of Styrofoam ALWA as a substitution to the coarse aggregate can reduce the density of concrete as much as 5 to 35%.
引用
收藏
页码:2011 / 2022
页数:12
相关论文
共 36 条
[1]   Evaluation of mechanical properties of steel fiber reinforced concrete with different strengths of concrete [J].
Abbass, Wasim ;
Khan, M. Iqbal ;
Mourad, Shehab .
CONSTRUCTION AND BUILDING MATERIALS, 2018, 168 :556-569
[2]  
ACI Committee 318, 2014, 318 ACI, V519
[3]  
Agustiar Tavio, 2018, INT J CIV ENG TECHNO, V9, P1249
[4]   Experimental Study of Cold - Bonded Artificial Lightweight Aggregate Concrete [J].
Ahmad, Hilfi Harisan ;
Tavio .
HUMAN-DEDICATED SUSTAINABLE PRODUCT AND PROCESS DESIGN: MATERIALS, RESOURCES, AND ENERGY, 2018, 1977
[5]  
Ahmad M. H., 2008, INT C CIV ENG MAY
[6]   Stress-Strain Relationship of High-Strength Steel (HSS) Reinforcing Bars [J].
Anggraini, Retno ;
Tavio ;
Raka, I. Gede Putu ;
Agustiar .
METALLURGY AND ADVANCED MATERIAL TECHNOLOGY FOR SUSTAINABLE DEVELOPMENT, 2018, 1964
[7]  
[Anonymous], 2018, C595C595M18 ASTM, DOI [10.1520/C0595_C0595M-18, DOI 10.1520/C0595_C0595M-18]
[8]  
[Anonymous], 2018, C3939M ASTM, DOI [10.1520/C0039_C0039M-18, DOI 10.1520/C0039_C0039M-18]
[9]   Ductile Structure Framework of Earthquake Resistant of Highrise Building on Exterior Beam-Column Joint with the Partial Prestressed Concrete Beam-Column Reinforced Concrete [J].
Astawa, Made D. ;
Tavio ;
Raka, I. G. P. .
2ND INTERNATIONAL CONFERENCE ON REHABILITATION AND MAINTENANCE IN CIVIL ENGINEERING (ICRMCE), 2013, 54 :413-427
[10]   MOMENT CONTRIBUTION CAPACITY OF TENDON PRESTRESSED PARTIAL ON CONCRETE BEAM-COLUMN JOINT INTERIOR ACCORDING TO PROVISIONS ACI 318-2008 CHAPTER 21.5.2.5(c) DUE TO CYCLIC LATERAL LOADS [J].
Astawa, Made Dharma ;
Raka, IGusti Putu ;
Tavio .
3RD BALI INTERNATIONAL SEMINAR ON SCIENCE & TECHNOLOGY (BISSTECH 2015), 2016, 58