COLD WORK EFFECTS ON SULFIDE STRESS CRACKING OF PIPELINE STEEL EXPOSED TO SOUR ENVIRONMENTS

被引:29
作者
HUANG, H
SHAW, WJD
机构
[1] Department of Mechanical Engineering, The University of Calgary, Calgary
关键词
D O I
10.1016/0010-938X(93)90259-J
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Cold work effects on sulfide stress cracking of a pipeline steel were examined for exposure to a sour gas environment. Cold worked steel was found to be sensitive to hydrogen embrittlement. The fracture toughness decreases with increasing cold work. Sufficiently low values of fracture toughness may be achieved to promote plane strain fracture even in relatively thin laboratory specimens after a steady state level of hydrogen has occurred in the material. Sulfide stress cracking failure of steel with low amounts of cold work (<30%) is by transgranular cleavage fracture, while heavily cold worked steel shows secondary cracks and microvoid coalescence. The results indicate that sulfide stress cracking of the steel is a mixture of anodic stress corrosion cracking (SCC) and hydrogen embrittlement. The anodic SCC mechanism is mainly promoted by carbon dioxide and a high level of chloride.
引用
收藏
页码:61 / 78
页数:18
相关论文
共 49 条
  • [1] THE THRESHOLD STRESS INTENSITY FOR HYDROGEN-INDUCED CRACK-GROWTH
    AKHURST, KN
    BAKER, TJ
    [J]. METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1981, 12 (06): : 1059 - 1070
  • [2] METALLURGICAL FACTORS CONTROLLING SSC RESISTANCE OF HIGH-STRENGTH, LOW-ALLOY STEELS
    ASAHI, H
    SOGO, Y
    UENO, M
    HIGASHIYAMA, H
    [J]. CORROSION, 1989, 45 (06) : 519 - 527
  • [3] Barba MJ, 1880, MEM SOC ING CIVILS 1, P682
  • [4] BEACHEM CD, 1972, METALL TRANS, V3, P437
  • [5] THE ROLE OF HYDROGEN IN SULFIDE STRESS CRACKING OF LOW-ALLOY STEELS
    BERKOWITZ, BJ
    HEUBAUM, FH
    [J]. CORROSION, 1984, 40 (05) : 240 - 245
  • [6] EFFECT OF IMPURITY SEGREGATION ON THE HYDROGEN EMBRITTLEMENT OF A HIGH-STRENGTH NICKEL-BASE ALLOY IN H2S ENVIRONMENTS
    BERKOWITZ, BJ
    KANE, RD
    [J]. CORROSION, 1980, 36 (01) : 24 - 29
  • [7] Birnbaum HK., 1979, ENV SENSITIVE FRACTU, P326
  • [8] BOCKRIS JO, 1973, MODERN ELECTROCHEMIS, V2, P1240
  • [9] HEAT-TREATMENT, PLASTIC-DEFORMATION, AND CORROSION OF LOW-CARBON STEEL
    CHANCE, RL
    [J]. CORROSION, 1977, 33 (03) : 108 - 113
  • [10] ROLE OF HYDROGEN IN THE DUCTILE FRACTURE OF PLAIN CARBON-STEELS
    CIALONE, H
    ASARO, RJ
    [J]. METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1979, 10 (03): : 367 - 375